Electrode pressure and weld time on MFDC spot welders
Nugget size is set by current, time and force together. On a medium-frequency inverter, changing the force without changing the schedule is the usual cause of inconsistent welds.
News & technical notes
Short, practical write-ups on process selection, machine setup and export preparation. Written for the engineer preparing a quote or the buyer checking a specification.

Nugget size is set by current, time and force together. On a medium-frequency inverter, changing the force without changing the schedule is the usual cause of inconsistent welds.

Mechanical stops set one mesh size per gantry. Servo positioning turns pitch into a recipe value, which changes how long a changeover actually takes.
Read the note
A seam that leaks usually has one section that ran too fast or with too little pressure, not a wrong current setting for the whole panel.
Read the note
Laser cells are not a general upgrade on spot welding. They win where the surface is visible, the part is thin, or the joint has to be continuous.
Read the note
Electrode tips, holders and shunts wear at different rates. A spares list matched to the machine model keeps a line running through the first year.
Read the noteNeed a specific answer
Send the material and the part, and the export desk will answer with the settings and the machine that suits them.