Technical article · 28 Oct 2026

Electrode pressure and weld time on MFDC spot welders

Nugget size is set by current, time and force together. On a medium-frequency inverter, changing the force without changing the schedule is the usual cause of inconsistent welds.

Close-up of a copper spot welding electrode tip

A spot weld forms in three stages: the electrodes clamp the sheets, current heats the interface, and the force is held while the nugget solidifies. On an MFDC machine the current rises quickly and stays flat, so force and time become the two settings that decide whether that nugget is sound or expelled.

If the electrode force is too low, contact resistance at the interface rises and the surface flashes before the nugget grows. The visible result is a dent with a ring of expelled metal and a nugget that fails a peel test. If the force is too high, the sheets are pressed thinner and current density drops, which produces a small nugget at the same schedule.

On galvanised and high-strength steel the window is narrower. Coating changes contact resistance at the start of the weld, so the schedule that suits bare steel usually needs a shorter weld time and a slightly higher current, with force set to keep the coating from being pushed away at the edge of the tip. That is why a schedule copied from another line rarely transfers without a coupon test.

The practical routine is the same for every part: weld a coupon of the exact material and thickness, cut or peel it, check nugget diameter against the drawing, then repeat after a shift of production to see how tip wear changes the result. Record the kA, time and force that passed, and the machine can be reset to those values after a tip change instead of being tuned by ear.

Technical support

Settings differ with material, thickness and fixture. Send your workpiece details and the export desk will reply with a starting parameter set.

Ask a question